NOTE: These values are representative values and do not relate to a specific grade of material
PNR - Polynorbornene Rubber
Glass Transition Temperature (°C) +25
Room Temperature Density (°C) 962
Maximum Working Temperature (°C) 100
Tensile Strength (MPa) M
Resistance To Tear M
Resistance To Abrasion M
Compression set @ -20°C (%) ---
Compression set @ +23°C (%) ---
Compression set @ +120°C (%) ---
Swelling / 70Hr / ASTM Oil No.3 @ 70°C (%) >140
Swelling / 70Hr / Fuel C @ Room Temperature (%) ---
Gas Permeability ---
Ozone Resistance M
Oxidation Resistance ---
Rebound (Hot) ---
Rebound (Cold) ---
Heat Resistance 5 Hours (°C) ---
Heat Resistance 70 Hours (°C) ---
Heat Resistance 1000 Hours (°C) ---
This information reproduced by kind permission of SkidMark Multimedia Productions. E-REF2 is a product of SkidMark Multimedia Productions. © 1994 - 2004