SBR
- Styrene Butadiene Rubber |
Glass
Transition Temperature (°C) |
-50 |
Room
Temperature Density (°C) |
912
<> 962 |
Maximum
Working Temperature (°C) |
110 |
Tensile
Strength (MPa) |
H |
Resistance
To Tear |
H |
Resistance
To Abrasion |
H |
Compression
set @ -20°C (%) |
--- |
Compression
set @ +23°C (%) |
--- |
Compression
set @ +120°C (%) |
--- |
Swelling
/ 70Hr / ASTM Oil No.3 @ 70°C (%) |
>140 |
Swelling
/ 70Hr / Fuel C @ Room Temperature (%) |
--- |
Gas
Permeability |
M |
Ozone
Resistance |
L |
Oxidation
Resistance |
M |
Rebound
(Hot) |
H |
Rebound
(Cold) |
H |
Heat Resistance
5 Hours (°C) |
195 |
Heat Resistance
70 Hours (°C) |
130 |
Heat Resistance
1000 Hours (°C) |
100 |
|
|